SABIC Lexan IR2240 High Flow
LEXAN™ IR2240 resin is a high-flow 11 MFR polycarbonate, MVR of 9. Grade designed for food contact applications. Mold release. Available in transparent, limited package types, and must meet minimum order quantity requirements.
- Character: 11 MFR, MVR of 9. Grade designed for food contact. Mold release.
Typical property data
Mechanical Properties
- Tensile Strength @ Yield: 62 MPa
- Flexural Modulus: 2,300 MPa
- Flexural Strength: 90 MPa
- Tensile Modulus: 2,300 MPa
- Elongation @ Break: 110%
Impact Properties
- Notched Izod Impact (23°C): 65 J/m
- Unnotched Izod Impact (23°C): No Break
Thermal Properties
- Heat Deflection Temp (1.8 MPa): 124°C
- Vicat Softening Temp (B/50): 147°C
Physical Properties
- Mold Shrinkage: 0.5 – 0.7%
- MVR (300°C/1.2kg): 9 cm³/10 min
- Density: 1.20 g/cm³
- Transparency: Yes
Flame Performance
- UL94 Flame Rating: V2 at 1.5 mm
Processing Guidelines
- Recommended Melt Temperature: 280 – 310°C
- Mold Temperature: 80 – 110°C
- Drying Conditions: 2 – 4 hours at 120°C
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin IR2240
LEXAN™ PC Resin IR1840
LEXAN™ PC Resin IR2210
LEXAN™ PC Resin IR2110
LEXAN™ PC Resin IR2040
LEXAN™ PC Resin IR1810
LEXAN™ PC Resin HFR1724
LEXAN™ PC Resin HF4010SR
LEXAN™ PC Resin HF3510R
LEXAN™ PC Resin HFR1723
LEXAN™ PC Resin HF1840R
LEXAN™ PC Resin HF1140R
LEXAN™ PC Resin HF1140
LEXAN™ PC Resin HF1130R
LEXAN™ PC Resin HF1130
LEXAN™ PC Resin HF1110R
LEXAN™ PC Resin HF1110
LEXAN™ PC Resin GLX143
Advanced Manufacturing