SABIC Lexan LS1 UV-stabilized
LEXAN™ Resin LS1 is a 20 MFR polycarbonate, MVR of 21. UL94 HB rated. UL746C f1 rated. UV-stabilized, low-viscosity polycarbonate designed for high-performance automotive lens applications. AMECA listed.
- Character: 20 MFR, MVR of 21. UL94 HB rated.
Typical property data
Mechanical Properties
- Tensile Strength at Yield: 60 MPa
- Flexural Strength: 90 MPa
- Flexural Modulus: 2,200 MPa
- Tensile Modulus: 2,200 MPa
Impact Properties
- Notched Izod Impact, 23°C: 65 J/m
- Unnotched Izod Impact, 23°C: No Break
Thermal Properties
- Heat Deflection Temperature (1.8 MPa): 125°C
- Vicat Softening Temperature: 145°C
- Coefficient of Thermal Expansion: 6.5 x 10⁻⁵ /°C
Physical Properties
- Melt Volume Rate (MVR) @ 300°C/1.2 kg: 21 cm³/10 min
- Density: 1.2 g/cm³
- Light Transmission: >88% (for 3.0 mm thickness)
Flame Performance
- UL94 Flame Rating: HB
- UL746C Outdoor Suitability: f1
Processing Guidelines
- Recommended Processing Temperature: 280°C – 320°C
- Mold Temperature: 80°C – 120°C
- Drying Conditions: 120°C for 4 hours
Download
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin LS1
LEXAN™ PC Resin IR2240
LEXAN™ PC Resin IR1840
LEXAN™ PC Resin IR2210
LEXAN™ PC Resin IR2110
LEXAN™ PC Resin IR2040
LEXAN™ PC Resin IR1810
LEXAN™ PC Resin HFR1724
LEXAN™ PC Resin HF4010SR
LEXAN™ PC Resin HF3510R
LEXAN™ PC Resin HFR1723
LEXAN™ PC Resin HF1840R
LEXAN™ PC Resin HF1140R
LEXAN™ PC Resin HF1140
LEXAN™ PC Resin HF1130R
LEXAN™ PC Resin HF1130
LEXAN™ PC Resin HF1110R
LEXAN™ PC Resin HF1110
Advanced Manufacturing