LEXAN™ PC Resin LS2

LEXAN™ PC Resin Sabic Tianjin

SABIC Lexan LS2 Flame Retardant Grade

LEXAN™ LS2 resin is a 11 MFR polycarbonate, MVR of 12. UV stabilized. UL94 HB rated. UL746C f1 rated. Medium viscosity. For Automotive lens applications. AMECA listed.

  • Character: 11 MFR, MVR of 12. UV stabilized. UL94 HB rated.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength @ Yield: 60 MPa
  • Flexural Strength: 90 MPa
  • Flexural Modulus: 2,300 MPa
  • Tensile Modulus: 2,200 MPa
  • Elongation @ Break: 110%

Impact Properties

  • Notched Izod Impact (23°C): 65 kJ/m²
  • Unnotched Izod Impact (23°C): No Break

Thermal Properties

  • Heat Deflection Temperature (1.8 MPa): 130°C
  • Vicat Softening Temperature: 147°C
  • Coefficient of Thermal Expansion: 6.5 x 10⁻⁵ /°C

Physical Properties

  • Melt Volume Rate (MVR, 300°C/1.2kg): 12 cm³/10 min
  • Density: 1.2 g/cm³
  • Light Transmission: >86%

Flame Performance

  • UL 94: HB Rated
  • UL 746C Outdoor Suitability: f1 Rated

Processing Guidelines

  • Recommended Melt Temperature: 280–310°C
  • Mold Temperature: 80–110°C
  • Drying Conditions: 120°C for 4 hours

Features & Benefits

UV-Stabilized for Outdoor Use

LEXAN LS2 resists yellowing and degradation from sunlight, making it ideal for exterior automotive lighting components.

High Optical Clarity

It delivers excellent light transmission, ensuring bright and consistent illumination in headlamp and signal lens applications.

AMECA Listed & UL Rated

It meets stringent automotive and safety standards, simplifying approval processes and ensuring regulatory compliance.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top