LEXAN™ PC Resin LUX1619

LEXAN™ PC Resin Sabic Tianjin

SABIC Lexan LUX1619 Flame Retardant Grade

LEXAN™ LUX1619 resin is a 7.5 MFR polycarbonate. UL94 HB rated. For high light reflectance. Extrudable and injection moldable.

  • Character: 7.5 MFR, UL94 HB rated.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength @ Yield: 61 MPa
  • Flexural Modulus: 2400 MPa
  • Flexural Strength: 90 MPa
  • Tensile Modulus: 2300 MPa
  • Elongation @ Break: 110%

Impact Properties

  • Izod Notched Impact (23°C): 65 J/m

Thermal Properties

  • Heat Deflection Temperature (1.8 MPa): 125°C
  • Vicat Softening Temperature: 148°C

Physical Properties

  • MFR (Melt Flow Rate): 7.5 g/10 min (300°C/1.2kg)
  • Specific Gravity: 1.19
  • Light Reflectance: High (optimized for LED and lighting applications)

Flame Performance

  • UL94 Flammability Rating: HB

Processing Guidelines

  • Processing Method: Extrusion and Injection Molding
  • Recommended Melt Temperature: 270–310°C
  • Mold Temperature: 80–110°C

Features & Benefits

High Light Reflectance

It can deliver superior brightness and diffusion, ideal for LED housings, backlit panels, and reflective lighting components.

Versatile Processing Options

Easily extrudable and injection moldable, allowing flexibility in part design and manufacturing across various production lines.

Dependable Thermal Stability

It can perform reliably at elevated temperatures (up to 125°C), suitable for demanding environments like enclosed lighting or electronic housings.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine