SABIC Lexan LUX2010T Injection Molding Grade

LEXAN™ Resin LUX2010T is a premium, global-grade polycarbonate designed for injection molding of optical parts. It offers outstanding flow properties, high light transmission, and excellent color stability—making it ideal for precision lighting and optical components.

  • Character: global-grade polycarbonate designed for injection molding of optical parts
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength at Yield: 60 MPa
  • Tensile Modulus: 2,300 MPa
  • Flexural Strength: 90 MPa
  • Flexural Modulus: 2,300 MPa

Impact Properties

  • Notched Izod Impact (23°C): 65 kJ/m²
  • Unnotched Izod Impact (23°C): No Break

Thermal Properties

  • Heat Deflection Temperature (1.8 MPa): 127°C
  • Vicat Softening Temperature (B/50): 144°C

Physical Properties

  • Light Transmission: >88%
  • Density: 1.2 g/cm³
  • Mold Shrinkage: 0.5 – 0.7%

Flame Performance

  • UL94 Rating: V2 at 1.5 mm and 3.0 mm

Processing Guidelines

  • Recommended Melt Temperature: 280 – 310°C
  • Mold Temperature: 80 – 120°C
  • Drying Conditions: 2 – 4 hours at 120°C

Features & Benefits

Exceptional Optical Clarity

LEXAN LUX2010T delivers over 88% light transmission—ideal for LED lenses, light guides, and optical housings.

Superior Flow for Complex Molds

Engineered for excellent flowability, this resin easily fills intricate mold geometries—reducing cycle times and improving surface finish.

Color Stability Over Time

It can maintain consistent color and clarity even under prolonged exposure to heat and light—critical for long-life lighting applications.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top