LEXAN™ Resin LUX2110T is a high-performance polycarbonate material engineered for precision optical parts. Designed for injection molding, it offers superior flow characteristics, excellent light transmission, and outstanding color stability.
- Character: Designed for injection molding, for precision optical parts
Typical property data
Mechanical Properties
- Tensile Strength at Yield: 60 MPa
- Tensile Modulus: 2,300 MPa
- Flexural Strength: 90 MPa
- Flexural Modulus: 2,300 MPa
- Rockwell Hardness (M scale): 75
Impact Properties
- Izod Notched Impact Strength (23°C): 65 kJ/m²
- Izod Notched Impact Strength (-30°C): 12 kJ/m²
Thermal Properties
- Heat Deflection Temperature (0.45 MPa): 138°C
- Vicat Softening Temperature (B/120): 145°C
- Coefficient of Linear Thermal Expansion: 6.5 x 10⁻⁵ /°C
Physical Properties
- Light Transmission: >88%
- Density: 1.2 g/cm³
- Mold Shrinkage: 0.5 – 0.7%
Flame Performance
- UL94 Rating (1.5 mm): V2
- Glow Wire Ignition Temperature (GWIT): 750°C
- Glow Wire Flammability Index (GWFI): 850°C
Processing Guidelines
- Recommended Mold Temperature: 80 – 110°C
- Melt Temperature: 280 – 310°C
- Drying Conditions: 120°C for 3–4 hours
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin LUX2619
LEXAN™ PC Resin LUX2614G
LEXAN™ PC Resin LUX2289
LEXAN™ PC Resin LUX2114G
LEXAN™ PC Resin LUX2114
LEXAN™ PC Resin LUX2110T
LEXAN™ PC Resin LUX2010T
LEXAN™ PC Resin LUX1619
LEXAN™ PC Resin LSHF
LEXAN™ PC Resin LS2
LEXAN™ PC Resin IR2840
LEXAN™ PC Resin LS1
LEXAN™ PC Resin IR2240
LEXAN™ PC Resin IR1840
LEXAN™ PC Resin IR2210
LEXAN™ PC Resin IR2110
LEXAN™ PC Resin IR2040
LEXAN™ PC Resin IR1810
Advanced Manufacturing