SABIC Lexan LUX2114 UV-stabilized

LEXAN™ Resin LUX2114 is a high-performance polycarbonate resin offering Improved flame retardance, UV stabilized, and internal mold release. With an 18 MFR, it’s ideal for LED lighting and electrical components requiring precision, safety, and durability.

  • Character: 18 MFR. Improved flame retardance. Internal mold release. UV stabilized.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength: 60 MPa
  • Flexural Modulus: 2,300 MPa
  • Elongation at Break: 110%

Impact Properties

  • Notched Izod Impact (23°C): 65 kJ/m²

Thermal Properties

  • Heat Deflection Temperature (1.8 MPa): 125°C
  • Vicat Softening Temperature: 145°C

Physical Properties

  • Melt Flow Rate (MFR): 18 g/10 min (300°C/1.2 kg)
  • Density: 1.2 g/cm³
  • UV Stabilized: Yes
  • Color: Transparent/Natural

Flame Performance

  • UL94 Flame Rating: V0 (1.5 mm and above)
  • Glow Wire Ignition Temperature (GWIT): ≥ 775°C

Processing Guidelines

  • Recommended Mold Temperature: 80–120°C
  • Drying Temperature: 120°C for 4 hours
  • Suggested Injection Temperature: 280–310°C

Features & Benefits

Superior Flame Retardance

LEXAN LUX2114 meets V0 rating at 1.5 mm, ensuring safety compliance in lighting and electrical housings.

UV-Stabilized for Outdoor Use

Engineered for long-term clarity and color retention in outdoor environments, ideal for LED lenses and covers.

Efficient Processing with Internal Mold Release

Built-in mold release reduces cycle times and tool wear—perfect for high-volume manufacturing of intricate parts.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top