Typical property data

Mechanical Properties

  • Tensile Strength @ Yield: 62 MPa
    Flexural Modulus: 2,340 MPa
    Flexural Strength @ Yield: 93 MPa

Impact Properties

  • Notched Izod Impact (23°C): 750 J/m
  • Unnotched Izod Impact (23°C): 3200 J/m
  • Falling Dart Impact (23°C): 169 J

Thermal Properties

  • Heat Deflection Temp @ 1.82 MPa: 132°C
  • Vicat Softening Temperature (Rate B/50): 154°C
  • Coefficient of Thermal Expansion: 6.84 x 10⁻⁵ /°C

Physical Properties

  • Density: 1.19 g/cm³
  • Water Absorption (24hrs): 0.15%
  • Mold Shrinkage: 0.5 – 0.7%

Flame Performance

  • UL94 Flame Rating: V-2 (0.75 – 1.65 mm)
  • Glow Wire Ignition Temperature (GWIT): 875°C @ 0.75mm
  • Glow Wire Flammability Index (GWFI): 850°C @ 1.5mm

Processing Guidelines

  • Injection Molding Melt Temp: 310–330°C
  • Mold Temperature: 80–115°C
  • Drying Temp/Time: 120°C for 3–4 hours

Features & Benefits

Superior Light Diffusion & Stability

This LEXAN LUX2614G resin delivers uniform light transmission and maintains color consistency even under prolonged heat, ensuring your LED products have a consistent, appealing appearance over time.

Built-in Safety with Flame Retardancy

The material meets key UL and IEC flame safety standards, reducing compliance complexity and helping you design safer LED lighting fixtures that protect end-users and mitigate risk.

Engineered for Molding Efficiency

With clear processing guidelines and good thermal stability, LEXAN Resin LUX2614G allows for streamlined injection molding, minimizing trial runs and boosting manufacturing yield for cost-effective production.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top