SABIC Lexan ML3729R UV-stabilized
LEXAN™ ML3729R resin is a 39 MFR polycarbonate, MVR of 36. UV stabilized. Mold release. UL94 V2 rated (US). Easy processing.
- Character: 39 MFR, MVR of 36. UV stabilized, UL94 V2 rated
Typical property data
Mechanical Properties
- Tensile Strength at Yield: 62 MPa
- Tensile Modulus: 2,410 MPa
- Flexural Strength at Yield: 101 MPa
- Flexural Modulus: 2,410 MPa
Impact Properties
- Izod Impact (Notched, 23°C): 686 J/m
- Charpy Impact (23°C, V-notch): 12 kJ/m²
Thermal Properties
- Heat Deflection Temperature (HDT @ 1.82 MPa): 124 °C
- Vicat Softening Temperature (Rate B/50): 139 °C
Physical Properties
- Specific Gravity: 1.2
- Melt Flow Rate (300°C/1.2kg): 39 g/10 min
- Water Absorption (Saturated): 0.27%
- Mold Shrinkage: 0.5 – 0.7%
Flame Performance
- UL94 Rating: V2 (US)
Processing Guidelines
- Drying: 120°C for 3-4 hours
- Melt Temperature: 270 – 295 °C
- Mold Temperature: 70 – 95 °C
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin ML3729R
LEXAN™ PC Resin ML3729
LEXAN™ PC Resin LUX2619
LEXAN™ PC Resin LUX2614G
LEXAN™ PC Resin LUX2289
LEXAN™ PC Resin LUX2114G
LEXAN™ PC Resin LUX2114
LEXAN™ PC Resin LUX2110T
LEXAN™ PC Resin LUX2010T
LEXAN™ PC Resin LUX1619
LEXAN™ PC Resin LSHF
LEXAN™ PC Resin LS2
LEXAN™ PC Resin IR2840
LEXAN™ PC Resin LS1
LEXAN™ PC Resin IR2240
LEXAN™ PC Resin IR1840
LEXAN™ PC Resin IR2210
LEXAN™ PC Resin IR2110
Advanced Manufacturing