SABIC Lexan OQ1022 optical Grade
LEXAN™ OQ1022 resin is an optical quality polycarbonate. High purity resin for CD, DVD and BD applications at short cycle times (not UV stabilized). Produced in dedicated equipment with stringent production control conditions.
- Character: optical-grade
Typical property data
Mechanical Properties
- Tensile Strength (Yield): 61 MPa
- Flexural Modulus: 2,460 MPa
- Flexural Strength: 93 MPa
- Tensile Modulus: ~2,420 MPa
Impact Properties
- Izod Impact (Notched): 550 J/m (ASTM) / 14 kJ/m² (ISO)
- Instrumented Dart Impact Total Energy: 46 J
- Charpy Impact (V-notch): 40 kJ/m²
Thermal Properties
- Heat Deflection Temperature (HDT @ 1.82 MPa): 123 °C
- Vicat Softening Temperature: 140 °C
- Coefficient of Thermal Expansion (CTE, flow): ~7.0E-05 1/°C
Physical Properties
- Specific Gravity / Density: 1.19
- Water Absorption (Saturated): 0.2%
- Mold Shrinkage (flow): 0.6 – 0.8%
Flame Performance
- Ball Pressure Test (75°C): Pass (NB – No Breakdown)
Processing Guidelines
- Drying: 120°C for 3-4 hours (≤0.02% moisture)
- Melt Temperature: 305 – 330 °C
- Mold Temperature: 65 – 95 °C
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin OQ1022
LEXAN™ PC Resin ML3729R
LEXAN™ PC Resin ML3729
LEXAN™ PC Resin LUX2619
LEXAN™ PC Resin LUX2614G
LEXAN™ PC Resin LUX2289
LEXAN™ PC Resin LUX2114G
LEXAN™ PC Resin LUX2114
LEXAN™ PC Resin LUX2110T
LEXAN™ PC Resin LUX2010T
LEXAN™ PC Resin LUX1619
LEXAN™ PC Resin LSHF
LEXAN™ PC Resin LS2
LEXAN™ PC Resin IR2840
LEXAN™ PC Resin LS1
LEXAN™ PC Resin IR2240
LEXAN™ PC Resin IR1840
LEXAN™ PC Resin IR2210
Advanced Manufacturing