LEXAN™ PC Resin OQ1028

LEXAN™ PC Resin Sabic Tianjin

SABIC Lexan OQ1028 optical Grade

LEXAN™ OQ1028 resin is an optical quality polycarbonate. High purity resin for CD, DVD and BD applications at short cycle times (not UV stabilized). Produced in dedicated equipment with stringent production control conditions.

  • Character: optical-grade
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength @ Yield: 60 MPa
  • Flexural Modulus: 2,300 MPa
  • Flexural Strength @ Yield: 90 MPa

Impact Properties

  • Izod Impact, Notched (+23°C): 15 kJ/m²
  • Izod Impact, Notched (-30°C): 12 kJ/m²

Thermal Properties

  • Heat Deflection Temperature (HDT) @ 1.82 MPa: 122 °C
  • Vicat Softening Temperature: 138 °C
  • Coefficient of Thermal Expansion (CTE): 7.0 x 10⁻⁵ /°C
  • Ball Pressure Test (125°C): Passes

Physical Properties

  • Specific Gravity / Density: 1.2
  • Light Transmission (2.54 mm): >90%
  • Haze (2.54 mm): <0.7%
  • Water Absorption (Saturated): 0.35%
  • Mold Shrinkage (Flow): 0.5 – 0.7%

Processing Guidelines

  • Melt Temperature Range: 340 – 370 °C
  • Recommended Mold Temperature: 75 – 95 °C
  • Drying Conditions: 120°C for 4-6 hours
  • Maximum Moisture Content: 0.02%

Features & Benefits

High Fluidity for Fast Cycles

The high melt flow rate enables faster injection speeds and shorter cycle times, increasing your production output and reducing manufacturing costs for optical media components.

Exceptional Optical Purity

With over 90% light transmission and extremely low haze, this plastic particles OQ1028 delivers the crystal-clear clarity required for precision optical applications, ensuring high-quality data readability in CDs, DVDs, and Blu-ray discs.

Superior Process Consistency

Produced under stringent controls, this resin offers reliable thermal stability and predictable mold shrinkage, resulting in consistent part dimensions, reduced waste, and stable performance in high-temperature molding environments.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top