LEXAN™ PC Resin OQ4005

LEXAN™ PC Resin Sabic Tianjin

SABIC Lexan OQ4005 Optical Grade

LEXAN™ OQ4005 is an optical-grade, UV-stabilized polycarbonate featuring superior clarity with a UV cut-off up to 400 nm and an MVR of 8. It is engineered to deliver exceptional optical purity and long-term weatherability, making it an ideal material for demanding applications like high-performance sunglass lenses and protective sunvisors.

  • Character: MVR of 8, UV-stabilized PC. Optical grade
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength at Yield: 64 MPa
  • Tensile Modulus: 2,300 MPa
  • Flexural Strength at Yield: 96 MPa
  • Flexural Modulus: 2,310 MPa

Impact Properties

  • Izod Impact, Unnotched (23°C): No Break (NB)
  • Izod Impact, Notched (23°C): 910 J/m

Thermal Properties

  • Vicat Softening Temperature: 145 °C
  • Heat Deflection Temperature (HDT @ 1.82 MPa): 129 °C
  • Coefficient of Thermal Expansion (CTE), flow: 6.06 x 10⁻⁵ /°C

Physical Properties

  • Specific Gravity: 1.2
  • Mold Shrinkage, flow: 0.77%
  • Water Absorption (saturated): 0.14%
  • Light Transmission (2.54 mm): 87%
  • Haze (2.54 mm): 0.4%

Flame Performance

  • Ball Pressure Test (125°C): Passes (IEC 60695-10-2)

Processing Guidelines

  • Drying: 120°C for 2-4 hours
  • Melt Temperature: 280 – 310 °C
  • Mold Temperature: 80 – 110 °C

Features & Benefits

Superior Optical Clarity & UV Protection

This LEXAN OQ4005 resin offers >87% light transmission with minimal haze, ensuring crystal-clear vision. Its built-in UV stabilizer blocks harmful rays up to 400 nm, significantly enhancing product longevity and user protection in outdoor applications.

Exceptional Durability and Impact Resistance

With a “No Break” rating in unnotched Izod tests, this material provides outstanding toughness and safety. This superior impact resistance of LEXAN Resin OQ4005 reduces breakage risks, ensuring reliable performance in demanding eyewear and visor components.

High Heat Resistance for Stable Performance

A Vicat softening point of 145°C ensures the resin maintains its shape and integrity under high temperatures. This thermal stability allows for use in environments where other plastics might warp, supporting consistent quality during both processing and end-use.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity