SABIC Lexan PK2870 UV-stabilized
LEXAN™ PK2870 resin is a 2.5 MFR branched polycarbonate, MVR of 2. High viscosity. For blow molding, with high melt strength and high impact resistance. Excellent candidate for water bottle applications. Available in transparent colors only.
- Character: 2.5 MFR, MVR of 2. High viscosity.
Typical property data
Mechanical Properties
- Tensile Strength at Yield: 62 MPa
- Flexural Modulus: 2,300 MPa
- Flexural Strength at Yield: 95 MPa
- Hardness, Rockwell R: 120
Impact Properties
- Izod Impact, Notched at 23°C: 750 J/m
- Falling Dart Impact at 23°C: 170 J
- Charpy Impact, Notched at 23°C: 70 kJ/m²
Thermal Properties
- Heat Deflection Temperature (HDT) at 1.82 MPa: 130°C
- Vicat Softening Temperature: 150°C
- Coefficient of Thermal Expansion (CTE): 7.0E-05 1/°C
Physical Properties
- Specific Gravity: 1.2
- Water Absorption (Saturated, 23°C): 0.35%
- Light Transmission (2.54 mm): 88%
- Haze (2.54 mm): <0.8%
- Melt Flow Rate (300°C/1.2kg): 2.5 g/10 min
Flame Performance
- UL Yellow Card Number: E207780-228450
- Ball Pressure Test (125°C): Pass
Processing Guidelines
- Drying Temperature: 120°C for 3-4 hours
- Melt Temperature Range: 320 – 345°C
- Mold Temperature Range: 80 – 115°C
Download
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin PK2870
LEXAN™ PC Resin OQ4820
LEXAN™ PC Resin OQ4320R
LEXAN™ PC Resin OQ4120R
LEXAN™ PC Resin OQ3820
LEXAN™ PC Resin OQ3420
LEXAN™ PC Resin OQ2720
LEXAN™ PC Resin OQ1028
LEXAN™ PC Resin OQ1022
LEXAN™ PC Resin ML3729R
LEXAN™ PC Resin ML3729
LEXAN™ PC Resin LUX2619
LEXAN™ PC Resin LUX2614G
LEXAN™ PC Resin LUX2289
LEXAN™ PC Resin LUX2114G
LEXAN™ PC Resin LUX2114
LEXAN™ PC Resin LUX2110T
LEXAN™ PC Resin LUX2010T
Advanced Manufacturing