SABIC Lexan PU1230R UV-stabilized
LEXAN™ PU1230R resin is a 11 MFR polycarbonate, MVR of 12. UV stabilized. Medium viscosity. Designed for Automotive trim applications, excellent PUR coating adhesion.
- Character: 11 MF, MVR of 12. UV stabilized.
Typical property data
Mechanical Properties
- Tensile Strength at Yield: 62 MPa
- Flexural Strength at Yield: 96 MPa
- Flexural Modulus: 2,340 MPa
Impact Properties
- Notched Izod Impact (23°C): 801 J/m
- Falling Dart Impact (23°C): 169 J
Thermal Properties
- Heat Deflection Temperature (1.82 MPa): 132°C
- Melt Temperature Range: 295 – 315°C
Physical Properties
- Specific Gravity: 1.20
- Water Absorption (24hrs): 0.15%
- Mold Shrinkage: 0.5 – 0.7%
- Light Transmission (2.54mm): 88%
Processing Guidelines
- Recommended Drying: 120°C for 3-4 hours
- Mold Temperature: 70 – 95°C
- Melt Flow Rate (300°C/1.2kg): 11 g/10 min
Download
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin PU1230R
LEXAN™ PC Resin PK2870
LEXAN™ PC Resin OQ4820
LEXAN™ PC Resin OQ4320R
LEXAN™ PC Resin OQ4120R
LEXAN™ PC Resin OQ3820
LEXAN™ PC Resin OQ3420
LEXAN™ PC Resin OQ2720
LEXAN™ PC Resin OQ1028
LEXAN™ PC Resin OQ1022
LEXAN™ PC Resin ML3729R
LEXAN™ PC Resin ML3729
LEXAN™ PC Resin LUX2619
LEXAN™ PC Resin LUX2614G
LEXAN™ PC Resin LUX2289
LEXAN™ PC Resin LUX2114G
LEXAN™ PC Resin LUX2114
LEXAN™ PC Resin LUX2110T
Advanced Manufacturing