LEXAN™ Resin T5R141RC is a high-performance engineering thermoplastic compound, formulated with 50% post-consumer recycled content as part of SABIC’s TRUCIRCLE™ portfolio. This 11 MFR polycarbonate offers excellent mechanical strength, high impact resistance, and inherent mold release, making it a robust and sustainable choice for demanding industrial components and durable goods.

  • Character: 11 MFR. Mold release.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength at Yield: 62 MPa
  • Tensile Strength at Break: 68 MPa
  • Flexural Strength at Yield: 99 MPa
  • Flexural Modulus: 2300 MPa

Impact Properties

  • Izod Impact, Notched (23°C): 750 J/m
  • Izod Impact, Unnotched (23°C): 3000 J/m

Thermal Properties

  • Heat Deflection Temperature (HDT @ 1.82 MPa): 130 °C
  • Vicat Softening Temperature: 150 °C
  • Coefficient of Thermal Expansion (CTE): 6.8E-05 1/°C

Physical Properties

  • Specific Gravity: 1.2
  • Mold Shrinkage: 0.5 – 0.7 %
  • Water Absorption (24 hrs): 0.35 %

Processing Guidelines

  • Melt Temperature: 295 – 315 °C
  • Mold Temperature: 70 – 95 °C
  • Drying Conditions: 120°C for 3-4 hours
  • Maximum Moisture Content: 0.02%

Features & Benefits

Sustainable Sourcing, Reduced Footprint

This LEXAN T5R141RC resin contains 50% post-consumer recycled plastic, helping you meet sustainability goals and reduce environmental impact without compromising on material performance.

Exceptional Toughness and Durability

With high notched and unnotched impact resistance, it ensures product longevity and reliability in demanding applications like automotive interiors, protective housings, and tool bodies.

Reliable and Efficient Processability

The material offers a balanced melt flow, wide processing window, and mold release properties, enabling faster cycle times, easier molding, and consistent high-quality part production.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top