SABIC Lexan VR2820 UV-stabilized
LEXAN™ Resin VR2820 is a high-performance, UV-stabilized polycarbonate engineered for demanding applications. It combines exceptional impact strength and thermal resistance with excellent clarity and built-in mold release, making it ideal for creating durable, transparent components through efficient injection molding.
- Character: 7 MFR, MVR of 6. UV stabilized. Mold release.
Typical property data
Mechanical Properties
- Tensile Strength at Yield: 63 MPa
- Tensile Strength at Break: 65 MPa
- Flexural Strength at Yield: 93 MPa
- Flexural Modulus: 2,300 MPa
Impact Properties
- Izod Impact, Notched (23°C): 900 J/m
Thermal Properties
- Heat Deflection Temperature (HDT @ 1.82 MPa): 124 °C
- Coefficient of Thermal Expansion (CTE): 6.84 x 10⁻⁵ /°C
Physical Properties
- Specific Gravity: 1.2
- Mold Shrinkage: 0.5 – 0.7 %
- Melt Flow Rate (MFR): 7 g/10 min
Flame Performance
- UL Recognized Component (UL Yellow Card): E121562-548558
Processing Guidelines
- Drying: 120°C for 3-4 hours (max 48 hrs cumulative)
- Melt Temperature: 310 – 330 °C
- Mold Temperature: 80 – 115 °C
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin VR2820
LEXAN™ PC Resin VR2220
LEXAN™ PC Resin VR2020
LEXAN™ PC Resin PU2030R
LEXAN™ PC Resin VR1820
LEXAN™ PC Resin T5R141RC
LEXAN™ PC Resin OQ4005
LEXAN™ PC Resin PU1230R
LEXAN™ PC Resin PK2870
LEXAN™ PC Resin OQ4820
LEXAN™ PC Resin OQ4320R
LEXAN™ PC Resin OQ4120R
LEXAN™ PC Resin OQ3820
LEXAN™ PC Resin OQ3420
LEXAN™ PC Resin OQ2720
LEXAN™ PC Resin OQ1028
LEXAN™ PC Resin OQ1022
LEXAN™ PC Resin ML3729R
Advanced Manufacturing