SABIC Lexan XLS1210 Automotive Optical Parts
LEXAN™ XLS1210 resin is a 18 MVR polycarbonate. Designed for automotive optical parts requiring very high transmission and color stability. AMECA listed for protected applications only.
- Character: 18 MVR
Typical property data
Mechanical Properties
- Tensile Strength @ Yield: 63 MPa
- Tensile Strength @ Break: 65 MPa
- Flexural Modulus: 2,300 MPa
- Flexural Strength @ Yield: 90 MPa
Impact Properties
- Notched Izod Impact @ 23°C: 65 kJ/m²
- Notched Izod Impact @ -30°C: 11 kJ/m²
- Unnotched Izod Impact: No Break (NB)
Thermal Properties
- Heat Deflection Temperature (HDT @ 1.8 MPa): 122 °C
- Vicat Softening Temperature (Rate B/120): 141 °C
- Relative Temperature Index (Electrical): 130 °C
- Coefficient of Thermal Expansion (CTE): 7.0E-05 1/°C
Physical Properties
- Density: 1.20 g/cm³
- Light Transmission (2.54 mm): >90%
- Haze (2.54 mm): <0.5%
- Water Absorption (Saturated): 0.35%
- Mold Shrinkage: 0.5 – 0.7%
Flame Performance
- Oxygen Index (LOI): 25%
- Glow Wire Flammability Index (850°C): Passes at 1 mm
Processing Guidelines
- Drying: 120°C for 2-4 hours
- Melt Temperature: 280 – 300°C
- Mold Temperature: 80 – 100°C
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin XLS1210
LEXAN™ PC Resin XLS1110T
LEXAN™ PC Resin XLS1110
LEXAN™ PC Resin VR2820
LEXAN™ PC Resin VR2220
LEXAN™ PC Resin VR2020
LEXAN™ PC Resin PU2030R
LEXAN™ PC Resin VR1820
LEXAN™ PC Resin T5R141RC
LEXAN™ PC Resin OQ4005
LEXAN™ PC Resin PU1230R
LEXAN™ PC Resin PK2870
LEXAN™ PC Resin OQ4820
LEXAN™ PC Resin OQ4320R
LEXAN™ PC Resin OQ4120R
LEXAN™ PC Resin OQ3820
LEXAN™ PC Resin OQ3420
LEXAN™ PC Resin OQ2720
Advanced Manufacturing