XENOY™ resin PC PBT 1103

SABIC® PC Resin

Xenoy PC PBT 1103

XENOY™ Resin 1103 by SABIC is a high-performance, impact-modified PBT+PC alloy engineered for demanding automotive applications. It delivers exceptional toughness at low temperatures and strong chemical resistance, available in gray and black, making it ideal for durable exterior and under-the-hood components.

  • Character: Unreinforced, impact modified PBT+PC alloy
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength at Yield: 51 MPa
  • Tensile Modulus: 1890 MPa
  • Flexural Strength at Yield: 77 MPa
  • Flexural Modulus: 1930 MPa

Impact Properties

  • Izod Impact (Notched, 23°C): 747 J/m
  • Izod Impact (Notched, -30°C): 530 J/m
  • Instrumented Dart Impact Total Energy (23°C): 61 J

Thermal Properties

  • HDT @ 1.82 MPa: 87 °C
  • Vicat Softening Temperature (Rate B/50): 125 °C
  • Coefficient of Thermal Expansion (Flow): 1.71E-04 1/°C

Physical Properties

  • Specific Gravity: 1.2
  • Density: 1.19 g/cm³
  • Mold Shrinkage (Flow): 0.8 – 1.0%
  • Water Absorption (Saturated): 0.2%

Processing Guidelines

  • Drying: 110°C for 4-6 hours
  • Melt Temperature: 255 – 275°C
  • Mold Temperature: 40 – 90°C

Features & Benefits

Superior Low-Temperature Toughness

XENOY 1103 maintains high impact strength down to -30°C, ensuring parts won’t brittle-crack in cold climates—critical for exterior trim and functional components.

Excellent Chemical & Environmental Resistance

It resists automotive fluids like oils and fuels, preventing degradation and preserving part integrity and appearance in under-hood and fuel system applications.

Predictable Processing & Molding

With clear drying and temperature guidelines, XENOY™ Resin 1103 ensures consistent flow, reduced waste, and high-quality surface finishes in complex molds.

VALOX™ FR PBT resin natual color

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity