XENOY™ resin PC PBT 1105

SABIC® PC Resin

Xenoy PC PBT 1105

XENOY™ Resin 1105 by SABIC is a high-performance, impact-modified PBT/PC blend designed for injection molding. It delivers excellent toughness even at sub-zero temperatures and offers very good paintability, making it an ideal engineering plastic for demanding exterior automotive components, industrial parts, and applications requiring durability and a Class-A finish.

  • Character: PBT/PC blend, injection molding grade
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength at Yield (ISO 527): 52 MPa
  • Tensile Modulus (ISO 527): 2070 MPa
  • Flexural Modulus (ISO 178): 2010 MPa
  • Flexural Strength at Yield (ISO 178): 78 MPa
  • Hardness, Shore D: 79

Impact Properties

  • Izod Impact, Notched @ 23°C: 755 J/m (ASTM)
  • Izod Impact, Notched @ -30°C: 489 J/m (ASTM)
  • Charpy Impact @ 23°C: 62 kJ/m² (ISO)

Thermal Properties

  • Heat Deflection Temp (HDT) @ 1.8 MPa: 90 °C
  • Vicat Softening Temperature: 122 °C

Physical Properties

  • Specific Gravity: 1.2
  • Mold Shrinkage: 0.8 – 1.0%
  • Melt Flow Rate (250°C/5.0 kg): 16 g/10 min

Processing Guidelines

  • Drying: 4-6 hours at 110°C
  • Melt Temperature: 260 – 275 °C
  • Mold Temperature: 65 – 90 °C

Features & Benefits

Exceptional Low-Temperature Toughness

The XENOY 1105 resin maintains high impact strength down to -40°C, ensuring parts won’t become brittle in cold environments. This reliability is critical for automotive exterior trim and components used in refrigerated or outdoor settings.

Superior Paint Adhesion and Finish

With its very good paintability, XENOY™ Resin 1105 readily accepts coatings without requiring primers, streamlining production. This results in a durable, high-quality finish perfect for painted automotive body panels and consumer electronics housings.

Balanced Stiffness and Processability

This non-reinforced blend offers an optimal balance of flexural modulus and easy flow for injection molding. It allows for the production of complex, thin-walled parts with good structural integrity and excellent surface appearance straight from the mold.

VALOX™ FR PBT resin natual color

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity