Sabic Cycoloy FR CY6110 (PC/ABS) Resin Cycoloy Fr resins CY6110 is a high-flow, flame-retardant PC/ABS blend. It offers exceptional impact strength and hydrostability, achieving a UL94 V-0 rating at just 1.5mm without using chlorinated or brominated flame retardants. Key technical data Download Application Features & Benefits Related CYCOLOY™ fR PC/ABS Products Advanced Manufacturing