Bayblend® W90 XG PC/ASA Resin General Purpose Grade Bayblend W90 XG is a premium PC+ASA blend engineered by Covestro for demanding applications. Offering exceptional UV stability, heat resistance (Vicat/B 120: 115°C), and superior surface finish, it excels in harsh environments while maintaining dimensional stability. Ideal for injection-molded parts requiring durability and aesthetics. Key technical data