Covestro Makrolon® 6265 X RE25 CQ

Makrolon 6265 X RE25 CQ PC Resin Makrolon 6265 X RE25 CQ is a low-viscosity, flame-retardant polycarbonate resin with UL 94V-0 certification (1.5 mm). Featuring easy-release molding (280–320°C melt temp), 19 cm³/10 min flow rate, and CQ renewable attribution via ISCC PLUS mass balance. Ideal for opaque-colored, high-safety applications demanding sustainability and efficiency. Key technical

Covestro Makrolon® 6265 X RE25 CQ Read More »

Covestro Makrolon® 6555 RE CQ

Makrolon 6555 RE CQ PC Resin Makrolon 6555 RE CQ is Covestro’s flame-retardant polycarbonate resin with medium viscosity (MVR 10 cm³/10 min) and UL 94V-0 certification (3.0 mm). Optimized for injection molding (280–320°C melt temp), it offers easy release, transparency/color versatility, and ISCC PLUS-certified bio-circular sustainability via mass balance. Key technical data (ISO) Download Application

Covestro Makrolon® 6555 RE CQ Read More »

Covestro Makrolon® 2856 RE CQ

Makrolon 2856 RE CQ PC Resin Partially Bio-circular Grade Makrolon® 2856 RE CQ is a medium-viscosity, food-contact-compliant polycarbonate resin with renewable content (CQ attribution). Featuring easy release and an MVR of 9.0 cm³/10 min (300°C/1.2 kg), it’s optimized for injection molding (280–320°C melt temp) and available in transparent/opaque colors. Key technical data (ISO) Download Application

Covestro Makrolon® 2856 RE CQ Read More »

Covestro Makrolon® 2456 RE CQ

Makrolon 2456 RE CQ PC Resin Bio-circular Grade Makrolon 2456 RE CQ is a low-viscosity polycarbonate resin offering easy mold release and versatile coloring (transparent/translucent/opaque). With an MVR of 19 cm³/10 min (300°C/1.2 kg), it ensures smooth processing and is food-contact-compliant. The CQ renewable attribution via ISCC PLUS mass balance supports sustainability goals without sacrificing

Covestro Makrolon® 2456 RE CQ Read More »

Covestro Makrolon® 6557 RE

Makrolon 6557 RE PC Resin Bio-circular Grade Makrolon® 6557 RE is a flame-retardant, UV-stabilized polycarbonate resin with medium viscosity and easy-release properties. It offers UL 94V-0 compliance at 3.0 mm thickness, bio-circular content via ISCC PLUS mass balance, and versatile color options (transparent/translucent/opaque). Ideal for high-safety injection-molded parts. Key technical data (ISO) Download Application Features

Covestro Makrolon® 6557 RE Read More »

Covestro Makrolon® 6487 RE

Makrolon 6487 RE PC Resin Flame Retardant Makrolon 6487 RE is a partially bio-circular polycarbonate resin (PC) with UL 94V-0/1.5mm and 5VA/3.0mm flame retardancy. Its medium viscosity, UV stabilization, easy-release properties, and opaque color options make it ideal for injection-molded safety-critical parts, combining sustainability (ISCC PLUS mass balance) with robust performance. Key technical data (ISO)

Covestro Makrolon® 6487 RE Read More »

Covestro Makrolon® 6267 X

Makrolon 6267 X PC Resin Flame Retardant Makrolon® 6267 X is a flame-retardant, low-viscosity polycarbonate resin with UL 94V-0 certification (1.5mm). Its easy-release properties, UV stabilization, and 19 cm³/10 min flow rate (300°C/1.2 kg) simplify injection molding of opaque safety-critical components like electrical housings. Key technical data (ISO) Download Application Features & Benefits Related Makrolon®

Covestro Makrolon® 6267 X Read More »

Covestro Makrolon® 6265 X

Makrolon 6265 X PC Resin flame Retardant Grade Makrolon® 6265 X is a flame-retardant, low-viscosity PC resin with excellent flow (MVR 19 cm³/10min) and UL 94V-0 compliance at 1.5mm. Ideal for complex injection molding, it ensures easy release and high safety in opaque applications. Key technical data (ISO) Download Application Features & Benefits Related Makrolon®

Covestro Makrolon® 6265 X Read More »

Covestro Makrolon® XT5010

Makrolon XT5010 PC Resin Makrolon® XT5010 by Covestro is an easy-processing, low-viscosity PC resin with a high melt flow (34 cm³/10 min) and excellent mold release. Featuring a 110°C Vicat softening point and transparent color options, it’s engineered for efficient injection molding of precision components like LCD TV frames. Key technical data (ISO) Download Application

Covestro Makrolon® XT5010 Read More »

Covestro Makrolon® GF9002

Makrolon GF9002 PC Resin Flame Retardant Covestro PC Makrolon GF9002 is a 10% glass fiber-reinforced, flame-retardant polycarbonate resin. With low viscosity (MVR 15 cm³/10 min) and UL 94V-0 certification at 1.2 mm, it ensures easy processing, excellent release, and safety for thin-wall electronic housings. Available exclusively in opaque colors. Key technical data (ISO) Download Application