Covestro Bayblend® W90 XG

Bayblend® W90 XG PC/ASA Resin General Purpose Grade Bayblend W90 XG is a premium PC+ASA blend engineered by Covestro for demanding applications. Offering exceptional UV stability, heat resistance (Vicat/B 120: 115°C), and superior surface finish, it excels in harsh environments while maintaining dimensional stability. Ideal for injection-molded parts requiring durability and aesthetics. Key technical data

Covestro Bayblend® W90 XG Read More »

Covestro Bayblend® W85 XF

Bayblend® W85 XF PC/ASA Resin Weather Resistant Grade Covestro Bayblend® W85 XF is a PC/ASA blend engineered for exceptional weather resistance, low-temperature toughness (-30°C), and reliable heat stability (Vicat 132°C). Perfect for outdoor and technical parts needing durability without compromising processability. Key technical data (ISO) Download Application Features & Benefits Related Apec® PC Resin Products