Kibilac® PW-997 Extrusion Grade Higher Flow ASA Resin
KIBILAC PW-997 is a high-quality ASA resin from CHIMEI. Perfect for outdoor use. It’s great for co-extrusion sheets and construction projects. The resin flows well and works nicely with PVC. It’s tough, resists heat, and can handle UV light. Whether you’re making window frames or outdoor furniture, this resin is a top choice for long-lasting, good-looking products.
- Application: Co-Extrusion sheet/Construction and outdoor application
- Character: Extrusion Grade,higher flow ability. Especially good compatibility with PVC.
Download
Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides. All documents are sourced directly from manufacturers.


Kibilac® PW-997 Datasheet
| Profile Extrusion ASA KIBILAC® PW-997 | ||||
| Product Description: Profile Extrusion | ||||
| Properties | ISO Test Method | Test Condition | Unit | PW-997 |
| Melt Flow Index | 1133 | 220℃×10KG | ml/10 min | 7 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.07 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 46 |
| 50 mm/min, break | MPa | 34 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 30 |
| Flexural Strength | 178 | 2 mm/min | MPa | 66 |
| Flexural Modulus | 178 | 2 mm/min | GPa | 2.1 |
| Izod Impact Strength | 180/1A | 23℃, Notched | KJ/m2 | 20 |
| -30℃, Notched | KJ/m2 | 9 | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 20.5 |
| -30℃, Notched | KJ/m2 | 10 | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 106 |
| 50℃/hr;5KG | ℃ | 94 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 79 |
| 1.8MPa, annealed | ℃ | 98 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 9.3×10-5 |
| Flammability | – | UL-94 | – | 1.5mm HB |
| Mold Shrinkage | 294-4 | – | % | 0.4~0.7 |
| Symbol | 1043 | – | – | >ASA< |
| 11-Mar-24 | ||||
Kibilac® PW-997 UL Product iQ
| KIBILAC® PW-997(++)(f1) UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Acrylonitrile Styrene Acrylate (ASA) “KIBILAC”, furnished as pellets |
| (++) – Optional suffix (except S and G) may be used to denote usage of 0-0.5 percent acid scavengers. | ||
| (f1) – Suitable for outdoor use with respect to exposure to Ultraviolet Light, Water Exposure and Immersion in accordance with UL 746C. | ||
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 1.5 mm, Color: ALL | HB | |
| 3.0 mm, Color: ALL | HB | |
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 1.5 mm, Color: ALL | HB75 | |
| 3.0 mm, Color: ALL | HB40 | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 1.5 mm | PLC 4 | |
| 3.0 mm | PLC 4 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 1.5 mm | PLC 2 | |
| 3.0 mm | PLC 2 | |
| Comparative Tracking Index (CTI) | PLC 2 | UL 746A |
| High Voltage Arc Tracking Rate (HVTR) | PLC 2 | |
| High Voltage, Low Current Arc Resistance | PLC 5 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 1.5 mm | 50 °C | |
| 3.0 mm | 50 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 1.5 mm | 50 °C | |
| 3.0 mm | 50 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 1.5 mm | 50 °C | |
| 3.0 mm | 50 °C | |
| PHYSICAL PROPERTIES | VALUE | TEST METHOD |
| UV Exposure & Water Immersion | f1 | UL 746C |
| Report Date: 2017-11-27 | ||
Advanced Manufacturing