CYCOLOY™ FR Resins C2950HF

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy FR C2950HF (PC/ABS) Resin

Cycoloy Fr resins C2950HF (PC/ABS) resin is a non-chlorinated, non-brominated flame retardant PC/ABS. This high-heat material offers enhanced processability and a superior UL V0 & 5VA/B flame rating for demanding applications.

  • Character: non-chlorinated, non-brominated flame retardant high heat
  • Application: appliances, lighting and electrical
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Flame Ratings: UL 94 V-0 (1.49mm), 5VA (3.4mm)
  • Heat Deflection Temp (HDT): 95 – 101°C (depending on load and thickness)
  • Tensile Strength at Yield: 64 MPa
  • Flexural Modulus: 2580 MPa
  • Izod Impact (Notched): 453 J/m
  • Relative Temperature Index (RTI): 85°C
  • Specific Gravity: 1.18
  • Melt Flow Rate: 22 g/10 min (260°C/2.16 kg)

Application

  • Appliances: Housings for power tools, internal components for large household appliances.
  • Lighting: LED light housings, diffusers, and electrical sockets.
  • Electrical: Electrical enclosures, connectors, and power distribution components.

Features & Benefits

Superior Flame Retardancy Without Halogens

This non-chlorinated, non-brominated flame retardant system meets strict UL V-0 and 5VA/B ratings, enabling compliance with global safety and environmental regulations for electronics and appliances.

Excellent Heat Resistance

With a Heat Deflection Temperature (HDT) up to 101°C, Cycoloy FR Resins C2950HF maintains structural integrity in high-heat environments, such as inside lighting fixtures or near power components.

Enhanced Processability and Impact Strength

This grade offers high flow and easier molding, reducing cycle times and improving productivity. Its high impact strength minimizes the risk of cracking during assembly and end-use.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity