CYCOLOY™ FR Resins C2951

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy FR C2951 (PC/ABS) Resin

Cycoloy FR Resins C2951 is a flame retardant PC/ABS resin engineered without chlorinated or brominated additives, offering a safer material choice for demanding electrical applications.

  • Character: flame retardant PC+ABS free from chlorinated or brominated flame retardant additives
  • Application: electrical applications
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Flame Ratings: UL 94 V-0 @ 1.5 mm
  • Flame Ratings: UL 94 5VB @ 2.5 mm
  • Flame Ratings: UL 94 SVA @ 3.0 mm
  • Heat Resistance: HDT @ 0.45 MPa: 103°C
  • Heat Resistance: HDT @ 1.82 MPa: 89°C
  • Vicat Softening Temperature: 109°C
  • Tensile Stress at Yield: 63 MPa
  • Flexural Modulus: 2550 MPa
  • Notched Izod Impact: 587 J/m
  • Melt Flow Rate: 10 g/10 min
  • Specific Gravity: 1.19
  • Mold Shrinkage: 0.4 – 0.6%

Application

  • Appliances: Internal components, housings, and connectors for large and small household appliances.
  • Lighting: Housings for LED fixtures, light diffusers, and electrical components requiring flame retardancy.
  • Electrical: Electrical enclosures, power distribution units, and connectors demanding high heat and impact resistance.

Features & Benefits

Superior Flame Retardancy, Halogen-Free

This PC/ABS resin achieves top UL-94 ratings without halogenated additives, ensuring regulatory compliance and a more environmentally conscious profile for your electronic housings and components.

High Heat Resistance & Durability

With a Heat Deflection Temperature of up to 103°C, it withstands high-temperature environments, preventing deformation in applications like internal lighting fixtures or appliance components near heat sources.

Excellent Impact Strength and Processability

It offers high notched Izod impact resistance, reducing part breakage, and a balanced melt flow for easy, efficient molding of complex, thin-walled parts, speeding up your production cycles.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity