Sabic Cycoloy FR C6600 (PC/ABS) Resin
Cycoloy FR RESINS C6600 is a flame-retardant, non-chlorinated/brominated thermoplastic blend offering excellent impact strength, chemical resistance, and hydrolytic stability. Ideal for opaque applications needing UL94 V0 performance and robust mechanical balance.
- Character: non chlorinated/brominated flame retardant grade with balanced flow, impact and hydrolytic stability. good chemical resistance and colorability in opaque colors.
- Application: injection moldable
Key technical data
- Flame Rating: UL94 V0 @ 1.5mm;
- Flame Rating: 5VB @ 2.0mm (non-halogenated)
- Tensile Strength: 50 MPa
- Flexural Modulus: 2,200 MPa
- Izod Notched Impact (23°C): 550 J/m
- Melt Flow Rate (260°C / 5kg): 8 g/10 min
- Heat Deflection Temp (1.82 MPa): 85°C
- Colorability: Excellent in opaque colors
- Hydrolytic Stability: High
- Chemical Resistance: Good
Application
- Electrical housings and enclosures
- Business equipment casings (printers, copiers, scanners)
- Consumer electronics (set-top boxes, routers, monitors)
- Automotive interior trim components
- Industrial control panels and instrument clusters
- Appliance parts requiring flame retardancy
- Medical device housings (non-implantable, external use)
- Battery packs and charging stations
- Power tools and handheld device casings
Features & Benefits

Related CYCOLOY™ fR PC/ABS Products
CYCOLOY™ FR Resins CY6414
CYCOLOY™ FR Resins CY6310
CYCOLOY™ FR Resins CY6120
CYCOLOY™ FR Resins CY6110
CYCOLOY™ FR Resins CY6025
CYCOLOY™ FR Resins CY5025
CYCOLOY™ FR Resins CM6240
CYCOLOY™ FR Resins CM6210
CYCOLOY™ FR Resins CM6220
CYCOLOY™ FR Resins CM6140
CYCOLOY™ FR Resins CE3510
CYCOLOY™ FR Resins C7230P
CYCOLOY™ FR Resins C6600
CYCOLOY™ FR Resins C6200
CYCOLOY™ FR Resins C3650
CYCOLOY™ FR Resins C2951
CYCOLOY™ FR Resins C2950HF
CYCOLOY™ FR Resins C2950
Advanced Manufacturing