Sabic Cycoloy FR CY6110 (PC/ABS) Resin

Cycoloy Fr resins CY6110 is a high-flow, flame-retardant PC/ABS blend. It offers exceptional impact strength and hydrostability, achieving a UL94 V-0 rating at just 1.5mm without using chlorinated or brominated flame retardants.

  • Character: an impact modified, high flow injection moldable, non chlorinated/brominated flame retardant grade
  • Application: Electrical Enclosures and Housings
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Flame Rating: UL94 V-0 (1.5 mm) | 5VB (2.5 mm)
  • Tensile Strength at Yield: 63 MPa
  • Tensile Modulus: 2760 MPa
  • Izod Impact (Notched, 23°C): 475 J/m²
  • Heat Deflection Temp (1.8 MPa): 88 °C
  • Melt Volume Rate (260°C/5.0 kg): 64 cm³/10 min
  • Relative Temperature Index (Elec/Mech): 85 °C
  • Density: 1.18 g/cm³
  • Ball Pressure Test (75°C): PASS

Application

  • Electrical Enclosures and Housings
  • Consumer Electronics Components
  • Automotive Interior Parts
  • Business Machine Housings
  • Connectors and Sockets
  • Charger Housings

Features & Benefits

Superior Flame Retardancy Without Halogens

This non-halogenated Flame Retardant PC+ABS Resin Cycoloy CY6110 meets strict safety standards (UL94 V-0 @ 1.5mm), enabling thinner, lighter, and more sustainable designs for electronics and enclosures.

Excellent Flow

The high flow nature of Cycoloy CY6110 resin ensures easy filling of intricate molds, reducing injection pressure and cycle times for higher productivity and lower manufacturing costs.

Outstanding Impact Strength and Durability

This impact-modified material maintains high toughness at room and low temperatures, ensuring your products can withstand accidental drops and physical stress throughout their lifecycle.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity

Scroll to Top