CYCOLOY™ FR Resins CY6120

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy FR CY6120 (PC/ABS) Resin

Cycoloy Fr resins CY6120 is a Non-chlorinated and non-brominated flame retardant PC/ABS. It offers excellent flow for thin walls and high impact strength, achieving UL94 V-0 at 1.2mm for demanding applications.

  • Character: Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties.
  • Application: thin wall applications
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Flame Rating: UL 94 V-0 (1.2 mm)
  • Melt Flow Rate (260°C/2.16 kg): 18 g/10 min
  • Tensile Strength at Yield: 62 MPa
  • Izod Impact (Notched): 587 J/m
  • Flexural Modulus: 2820 MPa
  • Heat Deflection Temp (1.82 MPa): 85 °C
  • Specific Gravity: 1.19

Application

  • Consumer electronics housings
  • Power supply covers
  • Automotive interior trim
  • Industrial control panels
  • Telecom enclosures
  • Thin-wall electrical components
  • Battery pack casings
  • Smart home device housings

Features & Benefits

Superior Flame Retardancy Without Halogens

This non-chlorinated, non-brominated Cycoloy CY6120 resin meets strict environmental and safety standards while providing reliable UL 94 V-0 protection at just 1.2mm thickness.

Excellent Flow

The high melt flow rate ensures easy filling of intricate and thin-walled parts, reducing injection pressure and improving production efficiency for complex components.

High Impact Strength and Durability

Outstanding Izod impact resistance ensures your products can withstand physical shocks and rough handling during use, enhancing product longevity and reliability.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity