Suke Plastics TPE 75N09

Suke Modified plastics TPE 75N09

Suke TPE 75N09 scratch resistance

Suke TPE 75N09 is a high-performance thermoplastic elastomer engineered for durability, offering a comfortable surface, scratch resistance, and exceptional size stability. Ideal for 3C electronics, kitchenware, and tool components, it combines flexibility with industrial-grade strength for demanding applications.

  • Manufacturer: Suke Plastics
  • Character: comfortable surface, scratch resistance, size stability
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Hardness:75 Shore A
  • Tensile Strength: 68.7 Kgf/cm²
  • Elongation at Break: 828%
  • Tear Strength: 46.5 Kgf/cm²
  • Melt Flow Rate: 10.79 g/10min
  • Processing Temp Range: 170–185°C
  • Pre-Drying: 80°C for 3 hours (simple prep for moisture-free molding).

Scratch-Resistant Surface

Suke TPE 75N09 resists daily wear and tear, maintaining a pristine finish on high-contact surfaces like smartphone cases or tool grips—ideal for industries valuing aesthetics and longevity.

Superior Flexibility & Strength

With 828% elongation and 68.7 Kgf/cm² tensile strength, this material bends without breaking, perfect for ergonomic kitchenware handles or stretchable electronic cable covers.

Stable Under Pressure

Boasts excellent size stability, ensuring parts retain shape during temperature shifts or heavy use—critical for precision-molded components in appliances and industrial tools.

Suke TPE 75N09

Application

  • IT & Communications: Server connectors, 5G router housings.
  • Electrical Appliances: Circuit breakers, switchgear components.
  • Household Appliances: Durable coffee machine gears, vacuum cleaner structural parts.
  • Industrial Electrical: Motor housings, relay insulators.
Suke Plastics TPE 75N09 application

Suke TPE 75N09 Datasheet

Suke TPE 75N09 Data Sheet
Product Description: comfortable surface, scratch resistance, size stability
Physical PropertiesTest StandardUnitsTypical Value
Pecific gravSPO-QC-001g/cm³1.127
HardnessSPO-QC-002shore75
Tensile strengthSPO-QC-003Kgf/cm³68.7
Elongation at breakSPO-QC-004%828
Tearing strengSPO-QC-005Kgf/cm³46.5
Melt indexgravitySPO-QC-006g/10min10.79
Processing conditionsRange
Pre-drying Conditions80℃,3 Hr
Nozzle   temp185℃
Screw 1 temp180℃
Screw 2 temp175℃
Screw 3 temp170℃

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top