Suke TPE 75N13 scratch resistance
Suke TPE 75N13 is a high-performance thermoplastic elastomer engineered for durability, offering a comfortable surface, scratch resistance, and exceptional size stability. Ideal for 3C electronics, kitchenware, and tool components, it combines flexibility with industrial-grade strength for demanding applications.
- Manufacturer: Suke Plastics
- Character: comfortable surface, scratch resistance, size stability
Key technical data (ISO)
- Hardness:75±3 Shore A
- Tensile Strength: 51.6 MPa
- Elongation at Break: 558%
- Tear Strength: 34.3 Kn/m
- Melt Flow Rate: 4.43 g/10min
- Processing Temp Range: 180–190°C
- Pre-Drying: 80°C for 3 hours
Download

Application
- IT & Communications: Server connectors, 5G router housings.
- Electrical Appliances: Circuit breakers, switchgear components.
- Household Appliances: Durable coffee machine gears, vacuum cleaner structural parts.
- Industrial Electrical: Motor housings, relay insulators.

Suke TPE 75N13 Datasheet
| Suke TPE 75N13 Data Sheet | |||
| Product Description: comfortable surface, scratch resistance, size stability | |||
| Physical Properties | Test Standard | Units | Typical Value |
| Pecific grav | ASTM D792 | g/cm³ | 1.112 |
| Hardness | ASTM D2240 | shoreA | 75±3 |
| Tensile strength | ASTM D412 | MPa | 51.6 |
| Elongation at break | ASTM D412 | % | 558 |
| Tearing streng | ASTM D624 | Kn/m | 34.3 |
| Melt indexgravity | ASTM D1238 | g/10min | 4.43 |
| Processing conditions | Range | ||
| Pre-drying Conditions | 80℃,3 Hr | ||
| Nozzle temp | 190℃ | ||
| Screw 1 temp | 185℃ | ||
| Screw 2 temp | 185℃ | ||
| Screw 3 temp | 180℃ | ||