VALOX™ FR PBT 364

SABIC® PC Resin

Valox FR PBT 364 Flame Retardant Grade

VALOX™ FR PBT 364 is a flame-retardant PBT plastic, offering superior impact strength and chemical resistance. It is UL94 V-0 rated at 1.47mm, making it an ideal, reliable choice for demanding outdoor telecom enclosures.

  • Character: unreinforced, impact modified flame retardant
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Flame Rating: UL 94 V-0 @ 1.47 mm / 5VA @ 3.0 mm
  • HDT @ 1.82 MPa: 68°C
  • Vicat Softening Point (B/50): 115°C
  • Tensile Strength at Break: 36 MPa
  • Flexural Modulus: 1800 MPa
  • Notched Izod Impact (23°C): 747 J/m
  • Specific Gravity: 1.3
  • Mold Shrinkage: 0.8 – 1.0%
  • Melt Flow Rate (266°C/5kg): 19 g/10 min
  • Melt Temperature: 250 – 265°C
  • Mold Temperature: 50 – 75°C
  • Drying: 3-4 hours at 120°C

Application

  • Outdoor Telecommunications Enclosures

Features & Benefits

Superior Flame Retardancy

This PBT VALOX 364 Resin achieves a UL94 V-0 rating at a thin 1.47mm, ensuring critical safety compliance and allowing for more compact, lightweight part designs in electrical applications.

Exceptional Impact Strength

With high notched Izod impact values, even at -40°C, this impact-modified material resists cracking from physical shocks and handles harsh outdoor environments with reliability.

Reliable Weather & Chemical Resistance

Excellent against moisture, UV light, and chemicals, this grade protects components long-term, making it a top candidate for outdoor telecommunications enclosures.

VALOX™ FR PBT resin natual color

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity