Valox FR PBT 780 Flame Retardant Grade
VALOX™ FR resin 780 is a flame-retardant PBT/PET plastic compound, reinforced with minerals and glass fibers. It offers superior electrical insulation, high mechanical strength, and a reduced blooming effect, making it a reliable and versatile choice for demanding electronic and electrical components.
- Character: mineral and glass fiber reinforced , reduced blooming effect, injection moldable grade.
Key technical data
- Flame Rating: UL 94 V-0 @ 0.81 mm
- Heat Resistance (HDT): 193°C @ 1.82 MPa
- Tensile Strength (Break): 99 MPa
- Flexural Modulus: 10,340 MPa
- Notched Izod Impact: 53 J/m
- Relative Temperature Index (Elec/Mech): 130°C / 140°C
- Specific Gravity: 1.77
- Volume Resistivity: 3.5E+15 Ω·cm
- Mold Shrinkage (Flow): 0.3 – 0.6%