Valox FR PBT 855 Flame Retardant Grade
VALOX™ FR resin 855 is a 15% glass-filled, flame-retardant PBT/PET compound. It offers a UL94 V-0 rating at 1.5mm, excellent chemical resistance, and superior aesthetics for demanding applications like appliances and lighting.
- Character: 15% glass filled, flame retardant
Key technical data
- Flame Rating: UL 94 V-0 @ 1.5 mm
- Heat Deflection Temp (HDT): 187°C @ 1.82 MPa
- Tensile Strength (Break): 95 MPa
- Flexural Modulus: 5000 MPa
- Notched Izod Impact: 55 J/m
- Relative Temperature Index (Elec): 125°C
- Specific Gravity: 1.5
- Mold Shrinkage (Flow): 0.4 – 0.6%
Download
Application
- Steam Irons (Base plates, housings)
- Appliance Components (Motor housings, connectors, handles)
- Lighting Parts (LED housings, reflectors, sockets)
Features & Benefits

Related Valox™ FR PBT Products
VALOX™ FR PBT V4860HR
VALOX™ FR PBT V4760
VALOX™ FR PBT V3900WX
VALOX™ FR PBT V3504
VALOX™ FR PBT SHF3800UX
VALOX™ FR PBT DR48
VALOX™ FR PBT 4631
VALOX™ FR PBT 4521
VALOX™ FR PBT 4512
VALOX™ FR PBT 3706
VALOX™ FR PBT 865
VALOX™ FR PBT 771
VALOX™ FR PBT 855
VALOX™ FR PBT 855
VALOX™ FR PBT 780
VALOX™ FR PBT 553U
VALOX™ FR PBT 457
VALOX™ FR PBT 420SE0
Advanced Manufacturing