VALOX™ FR PBT 865

SABIC® PC Resin

Valox FR PBT 865 Flame Retardant Grade

VALOX™ FR resin 865 is a 30% glass-filled, flame-retardant PBT/PET compound. It offers superior UL94 V-0 & 5VA ratings, excellent chemical resistance, and improved aesthetics, ideal for demanding electrical, appliance, and lighting components.

  • Character: 30% glass filled, flame retardant
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength (Break): 130 MPa
  • Flexural Modulus: 8,000 MPa
  • Notched Izod Impact: 80 J/m
  • HDT @1.82 MPa: 193 °C
  • Relative Temp Index (Elec/Mech): 110 °C
  • Flame Ratings UL 94 V-0: 1.5 mm
  • Flame Ratings UL 94 5VA: 3.0 mm
  • Specific Gravity: 1.66
  • Mold Shrinkage (Flow): 0.3 – 0.5%
  • Water Absorption (24hr): 0.03%

Application

  • Steam Irons & Garment Steamers: Bases and housings that resist high heat and steam.
  • Appliance Components: Housings and structural parts for toasters, coffee makers, and power tools.
  • Lighting Parts: Connectors, reflectors, and housings for both interior and exterior lighting systems.
  • Electrical Components: Circuit breakers, switches, and connectors requiring flame retardancy.

Features & Benefits

Superior Flame Retardancy & Safety

It meets stringent UL94 V-0 at 1.5mm and 5VA at 3.0mm, ensuring critical safety compliance and protecting your products and brand reputation in high-risk applications.

Exceptional Heat & Dimensional Stability

With a Heat Deflection Temperature of 193°C at 1.82 MPa, it maintains structural integrity and performance in high-heat environments like steam irons and appliance housings.

Reliable Electrical Insulation Properties

It boasts high volume resistivity and dielectric strength, providing consistent electrical insulation for components that must prevent short circuits and ensure user safety.

30% glass filled VALOX FR PBT resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top