FCFC Formosa TAIRILOY® AC3100

TAIRILOY AC3100

TAIRILOY® AC3100 Self Extinguishing Grade

TAIRILOY AC3100 PC/ABS Resin by FCFC is a halogen-free, flame-retardant alloy combining high flow and toughness. It offers UL compliance, V-0 flame resistance, and heat resistance. Features R110 hardness, 2350 MPa flexural modulus, and passes ball pressure tests. Engineered for durable, lightweight designs.

  • Manufacturer: FCFC (Formosa Chemicals & Fibre Corporation)
  • Application: Household appliances, 3C electronic products, notebook computers, Netcom products, computer peripheral products
  • Character: Flame retardant, Halogen free
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 21 g/10 min (260°C) – Excellent flow for complex molds.
  • Thermal Resistance: Vicat softening point @ 117°C – Retains shape under heat.
  • Flame Rating: V-0 (1.0–3.0mm), 5VA/5VB (2.3mm+) – Meets global safety standards.
  • Electrical Safety: PLC 0 for HAI/CTI – Minimizes arc risks in power components.
  • RTI (Electrical/Strength): Up to 90°C – Long-term reliability in heated environments.

Flame Retardant & Safe

AC3100 material achieves UL94 V-0 rating at 1.0mm thickness, ensuring compliance with strict safety standards. Ideal for circuit breaker housings or charger components where fire resistance is critical.

High Flow & Impact Resistance

With 21g/10min melt flow and 540 J/m impact strength, it enables thin-walled designs for laptops and netcom devices without sacrificing durability.

Dimensional Stability

Low molding shrinkage (0.4–0.6%) and high flexural modulus (2,350 MPa) ensure tight tolerances for intricate parts like thin-wall connectors or appliance panels.

TAIRILOY AC3100 PC ABS Resin

Applications

  • Household Appliances: Flame-retardant housings for coffee makers, hairdryers.
  • 3C Electronics: Smartphone cases, tablet frames, and charger plugs.
  • Notebook Computers: Lightweight yet impact-resistant laptop bodies.
  • Netcom Products: Router enclosures, modem casings.
  • Computer Peripherals: Keyboards, printer components, and thin-wall connectors.
TAIRILOY AC3100 application

Tairiloy® AC3100 Datasheet

General Purpose Grade FCFC TAIRILOY® AC3100 Data Sheet
Product Description: Metal plating
PropertyUnitTest MethodTest ConditionModel AC3100
Melt Flow Indexg/10 minISO 1133260℃ × 5kg21
IZOD Impact StrengthJ/mISO 18023 ℃ 3.2mm540
Charpy Impact StrengthkJ/m²ISO 17923 ℃ 4mm40
Specific GravityISO 118323℃/23℃1.08
Flexural StrengthMpaISO 17823 ℃86
Flexural ModulusMpaISO 17823 ℃2350
Rockwell HardnessR-scaleISO 2039-223℃R-110
Vicat Softening PointISO 306VICAT(10N ℃)117
Molding Shrinkage%ISO 25773.2mm0.4 ~ 0.6
CombustibilityUL-94File No. E162823HB 1.5 ~ 1.65 mm
All tests were run under laboratory conditions, ASTM, ISO testing procedures.
The data are intended as a general guide only.
Formosa Chemicals & Fibre Corp. Plastics Div.

Tairiloy® AC3100 UL Product iQ

TAIRILOY® AC310(+) UL Product iQ
File Number: E162823Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS), pellets
(+) – Replace by one digital 0-9 or one alphabet A-Z, unconcerned with formula or constituent changed
FlammabilityValueTest Method
Flame RatingUL 94
0.8 mm, ALLV-2IEC 60695-11-10, -20
1.0 mm, ALLV-0
1.2 mm, ALLV-0
1.5 mm, ALLV-0
2.3 mm, ALLV-0, 5VB
3.0 mm, ALLV-0, 5VA
ElectricalValueTest Method
Hot-wire Ignition (HWI)UL 746
0.8 mmPLC 3
1.0 mmPLC 3
1.2 mmPLC 3
1.5 mmPLC 3
2.3 mmPLC 2
High Amp Arc Ignition (HAI)UL 746
0.8 mmPLC 0
1.0 mmPLC 0
1.2 mmPLC 0
1.5 mmPLC 0
2.3 mmPLC 0
Comparative Tracking Index (CTI)PLC 0UL 746
High Voltage Arc Tracking Rate (HVTR)PLC 3UL 746
Arc ResistancePLC 7ASTM D495
ThermalValueTest Method
RTI ElecUL 746
0.8 mm60.0°C
1.0 mm60.0°C
1.2 mm60.0°C
1.5 mm90.0°C
2.3 mm90.0°C
3.0 mm90.0°C
RTI ImpUL 746
0.8 mm60.0°C
1.0 mm60.0°C
1.2 mm60.0°C
1.5 mm85.0°C
2.3 mm85.0°C
3.0 mm85.0°C
ThermalValueTest Method
RTI StrUL 746
0.8 mm60.0°C
1.0 mm60.0°C
1.2 mm60.0°C
1.5 mm90.0°C
2.3 mm90.0°C
3.0 mm90.0°C
Ball Pressure Test (75°C, 3.00 mm)PassIEC 60695-10-2

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top