TAIRILOY® AC2300 PC ABS Resin General Grade
TAIRILOY AC2300 by Formosa Plastics is a versatile General Purpose Grade PC/ABS alloy ideal for metal-plated applications. It offers excellent impact resistance, high flexural strength, and heat tolerance. With a melt flow index of 9–21g/10min. UL94 HB fire rating ensures safety, while low shrinkage reduces post-molding issues. Perfect for durability and cost-effective production.
- Application: Auto parts, household appliances, 3C electronic products and household goods casings such as wheel covers, handles, Portable storage device
 - Character: Metal plating
 
Key technical data (ISO)
- Impact Strength: 540 J/m (IZOD, 23°C) / 40 kJ/m² (Charpy)
 - Thermal Stability: Vicat Softening Point 117°C; RTI 60°C (Electrical/Mechanical)
 - Flow & Molding: Melt Flow Index 9–21g/10min; Shrinkage 0.4–0.6%
 - Safety Compliance: UL94 HB Flame Rating (1.5–1.7mm); Arc Resistance PLC 6
 - Weight & Hardness: Specific Gravity 1.08; Rockwell Hardness R-110
 
Features & Benefits

Application

Tairiloy® AC2300 Datasheet
| General Purpose Grade FCFC TAIRILOY® AC2300 Data Sheet | ||||
| Product Description: Metal plating | ||||
| Property | Unit | Test Method | Test Condition | Model AC2300 | 
| Melt Flow Index | g/10 min | ISO 1133 | 240℃ × 5kg | 9 | 
| Melt Flow Index | g/10 min | ISO 1133 | 260℃ × 5kg | 21 | 
| IZOD Impact Strength | J/m | ISO 180 | 23 ℃ 3.2mm | 540 | 
| Charpy Impact Strength | kJ/m² | ISO 179 | 23 ℃ 4mm | 40 | 
| Specific Gravity | – | ISO 1183 | 23℃/23℃ | 1.08 | 
| Flexural Strength | Mpa | ISO 178 | 23 ℃ | 86 | 
| Flexural Modulus | Mpa | ISO 178 | 23 ℃ | 2350 | 
| Rockwell Hardness | R-scale | ISO 2039-2 | 23℃ | R-110 | 
| Vicat Softening Point | ℃ | ISO 306 | VICAT(10N ℃) | 117 | 
| Molding Shrinkage | % | ISO 2577 | 3.2mm | 0.4 ~ 0.6 | 
| Combustibility | UL-94 | File No. E162823 | HB 1.5 ~ 1.65 mm | |
| All tests were run under laboratory conditions, ASTM, ISO testing procedures. | ||||
| The data are intended as a general guide only. | ||||
| Formosa Chemicals & Fibre Corp. Plastics Div. | ||||
Tairiloy® AC2300 UL Product iQ
| TAIRILOY® AC230(+) UL Product iQ | ||
| File Number: E162823 | Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS), pellets | |
| (+) – Replace by one digital 0-9 or one alphabet A-Z, unconcerned with formula or constituent changed. | ||
| Flammability | Value | Test Method | 
| Flame Rating | ||
| 1.5 to 1.7 mm, ALL | HB | UL 94 | 
| 1.5 to 1.7 mm, ALL | HB75 | IEC 60695-11-10, -20 | 
| Electrical | Value | Test Method | 
| Hot-wire Ignition (HWI) (1.5 to 1.7 mm) | PLC 4 | UL 746 | 
| High Amp Arc Ignition (HAI) (1.5 to 1.7 mm) | PLC 0 | UL 746 | 
| Comparative Tracking Index (CTI) | PLC 0 | UL 746 | 
| High Voltage Arc Tracking Rate (HVTR) | PLC 2 | UL 746 | 
| Arc Resistance | PLC 6 | ASTM D495 | 
| Thermal | Value | Test Method | 
| RTI Elec (1.5 to 1.7 mm) | 60.0°C | UL 746 | 
| RTI Imp (1.5 to 1.7 mm) | 60.0°C | UL 746 | 
| RTI Str (1.5 to 1.7 mm) | 60.0°C | UL 746 | 
Advanced Manufacturing