TAIRIREX® GP5350 GPPS Resin General Grade
TAIRIREX GP5350 is a high-heat-resistant general-purpose polystyrene (GPPS) resin in pellet form, designed for demanding applications requiring durability, clarity, and thermal stability. With superior heat deflection and mechanical performance, it’s ideal for kitchenware, lighting, and consumer goods where reliability under stress matters.
- Manufacturer: FCFC (Formosa Chemicals & Fibre Corporation)
- Character: High heat resistance
- Application: Kitchen ware, Lamp covers, Decorated sheets, Toys
Key technical data (ISO)
- Melt Flow Index: 4.5 g/10min (200°C, 5kg)
- Impact Strength: 1.6 kJ/m² (IZOD, unnotched) | 10.8 kJ/m² (Charpy)
- Tensile Strength: 44 MPa | Flexural Strength: 76 MPa
- Heat Resistance: Vicat Softening Point 100°C | Heat Deflection Temp. 95°C
- Safety: UL 94 HB rated (1.5–1.7 mm thickness)
- Residual Monomer: ≤700 ppm