FCFC Formosa TAIRIREX® GP5500

FCFC TAIRIREX GPPS Resin

TAIRIREX® GP5500 GPPS Resin General Grade

With a melt flow index of 2.6 g/10min, TAIRIREX GP5500 ensures rapid production cycles while maintaining excellent clarity, rigidity, and UL 94 HB flammability certification. Ideal for applications requiring precision and durability, this Formosa GPPS GP5500 resin balances processability with reliable mechanical performance.

  • Manufacturer: FCFC (Formosa Chemicals & Fibre Corporation)
  • Character: High molecular weight
  • Application: PSP sheets, OPS,Medicine containerss
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 2.6 g/10min (200°C, 5kg)
  • Impact Strength: 1.6 kJ/m² (IZOD, unnotched) | 9.5 kJ/m² (Charpy)
  • Tensile Strength: 47 MPa | Flexural Strength: 85 MPa
  • Thermal Resistance: Vicat Softening Point 103°C | HDT 98°C (1.8MPa)
  • Safety Compliance: UL 94 HB flame rating (1.5–1.7mm thickness)

Features & Benefits

Superior Flow for Complex Molds

High flow rate reduces cycle times, enabling cost-effective mass production of thin-walled or intricate parts without compromising structural integrity.

Enhanced Impact Resistance

With 1.6 kJ/m² IZOD and 9.5 kJ/m² Charpy impact strength, this PS resin minimizes brittleness, ensuring durability in everyday handling and assembly processes.

Thermal Stability Under Stress

A Vicat softening point of 103°C and heat deflection temperature (HDT) of 98°C allow consistent performance in high-temperature environments, such as sterilized medical tools.

FCFC Formosa TAIRIREX GPPS Resin

Application

PSP Sheets

Ideal for rigid, transparent food packaging due to excellent clarity and dimensional stability.

OPS Films

Used in shrink-wrap labels for bottles, leveraging high gloss and easy processability.

Withstands autoclaving and resists stress cracking, ensuring safe storage for pharmaceuticals.

Tairirex GP5500 application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top