TAIRISAN® NF2200
TAIRISAN NF2200 is a high-performance Styrene Acrylonitrile resin (SAN) engineered by Formosa Chemicals. Combining high heat resistance (Vicat 101°C) and excellent chemical stability, this injection-grade material excels in precision parts like fan blades and battery housings, offering durability and dimensional accuracy.
- Manufacturer: FCFC (Formosa Chemicals & Fibre Corporation)
- Character: High heat, Chemical resistance
- Application: Trash cans, Toothbrush handles, Lamp covers, Pen tube, Cup with cover, Cosmetic cases
Key technical data (ISO)
- Melt Flow Index (220°C/10kg): 29 g/10 min (ISO 1133)
- Tensile Strength: 73 MPa (ISO 527)
- Flexural Modulus: 3,600 MPa (ISO 178)
- Heat Deflection Temp (1.8MPa): 102°C (ISO 75/A)
- Vicat Softening Point: 101°C (ISO 306)
- Combustibility Rating: HB (UL 94, 1.5mm thickness)
- Molding Shrinkage: 0.4–0.7% (ISO 2577)
Features & Benefits

Application

Related Tairisan® SAN Plastics