TAIRILAC® WF3301 Weathering Grade ASA Resin
Tairilac WF3301 is a high-performance engineering plastic – ASA Resin. With exceptional UV resistance, color stability, and durability, this high-flow grade material ensures long-lasting performance in harsh environments. Ideal for automotive parts, outdoor piping, and HVAC components, it combines weather resilience with easy processing for industrial efficiency.
- Manufacturer: FCFC (Formosa Chemicals & Fibre Corporation)
- Character: Weather resistance is excellent, Color stable, Suitable for outdoor use
- Application: Fans of air-conditioner, Parts of car, Outside pipes
Key technical data (ISO)
- Melt Flow Index: 30 g/10min (220°C, 10kg)
- Charpy Impact Strength: 24 kJ/m² (23°C, notched)
- Tensile Strength: 38 MPa
- Flexural Strength: 53 MPa
- Heat Deflection Temperature: 90°C (1.8MPa)
- Flame Rating: HB (UL 94)
- Outdoor Suitability: Certified for UV, water, and immersion resistance (UL 746C)