FCFC Formosa TAIRILAC® WE8303

FCFC Tairilac ASA resin

TAIRILAC® WE8303 Weathering Grade ASA Resin

Tairilac WE8303 is a high-performance ASA resin, designed for extrusion applications requiring excellent weather resistance and long-term durability. Ideal for outdoor products, this material retains color and strength under harsh environmental conditions.

  • Manufacturer: FCFC (Formosa Chemicals & Fibre Corporation)
  • Character: Excellent weather resistance, Extrusion products
  • Application: Outdoor Products, junction box, Auto parts
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Rate (MFR): 5.0 g/10min (ISO 1133, 220°C/10kg)
  • Tensile Strength: 42 MPa (ISO 527)
  • Flexural Strength: 65 MPa (ISO 178)
  • Flexural Modulus: 1900 MPa (ISO 178)
  • Izod Notched Impact Strength (23°C): 35 kJ/m² (ISO 180)
  • Heat Deflection Temperature (1.8 MPa): 86°C (ISO 75)
  • UL Certification: UL 94 HB

Features & Benefits

Superior Weather Resistance

Tairilac WE8303 resin withstands prolonged UV exposure and extreme temperatures without cracking or fading, ideal for outdoor products like signage and roofing.

High Impact StrengthRobu

With a Charpy Impact Strength of 34 kJ/m², this resin resists mechanical stress, reducing breakage in automotive components and protective housings.

Thermal Stability

A Vicat Softening Point of 93°C ensures dimensional stability in high-heat environments, perfect for electrical enclosures and automotive under-the-hood parts.

FCFC Tairilac ASA resinparticles

Application

Outdoor Products:

Solar panel frames, garden equipment, and signage due to UV and moisture resistance.

Junction Boxes:

It can protect electrical components with flame-retardant (HB) and insulating properties.

Auto Parts:

Exterior trims, mirror housings, and grilles benefiting from impact resistance and color retention.

Tairilac ASA resin WE8303 application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top