FCFC Formosa TAIRILAC® WE830M

FCFC Tairilac ASA resin

TAIRILAC® WE830M Weathering Grade ASA Resin

Tairilac WTAIRILAC WE830M ASA Resin from FCFC is a high-performance engineering plastic designed for demanding outdoor applications. With exceptional weather resistance and UV stability, this material is ideal for modified plastic roof tiles and other exterior components.E830M

  • Character: Excellent weather resistance, Suitable for plastic roof tile modified use.
  • Application:Suitable for plastic roof tile modified use.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 10 g/10 min (200°C, 5kg)
  • Impact Strength: 11 kJ/m² (Charpy, notched, 23°C)
  • Specific Gravity: 1.05 (water = 1)
  • Heat Resistance: Vicat Softening Point 87°C; Heat Deflection Temp 88°C (1.8 MPa)
  • Molding Shrinkage: 0.4–0.7% (3.2mm thickness)

Features & Benefits

Superior Weather Resistance

Tairilac WE830M withstands harsh UV exposure and extreme temperatures without fading or cracking, ensuring long-term performance in outdoor environments like roofing systems.

High Mechanical Strength

With a tensile strength of 29 MPa and flexural modulus of 1,400 MPa, this FCFC ASA Resin delivers structural integrity for load-bearing applications, reducing material failure risks.

Easy Processing&Consistency

Pre-drying at 80–85°C (2–3 hours) and compatibility with extrusion/injection molding streamline production, minimizing downtime and ensuring uniform product quality.

FCFC Tairilac ASA resinparticles

Application

Plastic Roof Tiles

Modified for enhanced UV resistance and durability in roofing systems.

Outdoor Construction Profiles

Ideal for fascia, cladding, and trim exposed to weathering.

Automotive Exteriors

Suitable for non-structural parts requiring color retention and impact resistance.

Tairilac ASA resin WE830M application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top