Covestro Makrolon® AL2447 RE

Makrolon PC Polycarbonate

Makrolon AL2447 RE Polycarbonate Granules

Makrolon® AL2447 RE by Covestro is a low-viscosity, UV-stabilized polycarbonate resin ideal for injection molding. Featuring easy mold release and exceptional optical clarity (89% light transmission at 1mm), it’s available in transparent and signal colors. This ISCC PLUS-certified bio-circular grade supports sustainability goals without compromising performance.

  • Character: MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; UV stabilized; easy release; available in clear transparent colors and in various signal colors. CQ renewable attributed, Optical quality
  • Application: Injection molding; General purpose
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flow Rate: 19 cm³/10 min (300°C, 1.2 kg)
  • HDT @1.8 MPa: 125°C | @0.45 MPa: 138°C
  • Vicat Softening: 144°C
  • Tensile Modulus: 2,400 MPa | Flexural Strength: 98 MPa
  • Notched Impact (Charpy, -30°C): 14 kJ/m²
  • Refractive Index: 1.586 | Haze: <0.5% (3mm)
  • CTI: 250 (Tracking Resistance) | Volume Resistivity: 1E14 Ω·m
  • Melt Temp: 280–320°C | Mold Temp: 80–120°C
  • Drying: 120°C for 2–3 hrs (≤0.02% moisture)

Application

  • Automotive Headlamp Lenses: UV-resistant clarity for long-lasting forward lighting.
  • Signal Lighting: Vibrant colors for traffic indicators/emergency systems.
  • Optical Components: Thin-wall lenses, covers, and displays requiring scratch resistance.
  • Industrial Housings: Durable enclosures for electrical/electronic parts.
  • Consumer Goods: Transparent casings for appliances and wearables.

Features & Benefits

Eco-Friendly Material Choice

Partially bio-circular via mass balance (ISCC PLUS), reducing carbon footprint while maintaining high-performance standards for eco-conscious manufacturing.

Superior Optical Clarity

It delivers >87% luminous transmittance (even at 4mm thickness) and <0.5% haze, ensuring crystal-clear visibility for precision lighting components.

Optimized Processing Efficiency

Low viscosity (19 cm³/10 min MVR) and easy-release properties cut cycle times and energy use, streamlining high-volume injection molding.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top