Covestro Makrolon® AL2647 RP70 CQ

Makrolon PC Polycarbonate

Makrolon AL2647 RP70 CQ Polycarbonate Granules

Makrolon AL2647 RP70 CQ is a UV-stabilized, partially circular polycarbonate resin made from post-consumer recycled content via ISCC PLUS mass balance. Designed for automotive lighting, it offers exceptional optical clarity, easy release, and injection molding versatility in transparent/signal colors.

  • Character:
  • Application:
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flow Rate (MVR): 12 cm³/10 min (300°C/1.2 kg)
  • Tensile Modulus: 2,400 MPa
  • Yield Stress: 67 MPa
  • Notched Impact (23°C): 70 kJ/m²
  • HDT (1.8 MPa): 123°C
  • Vicat Softening: 143°C
  • Transmittance: 89% (1mm thickness)
  • Haze: <0.5% (3mm)
  • CTI: 250 (Comparative Tracking Index)
  • Volume Resistivity: 1E14 Ω·m

Application

  • Headlamp lenses (forward lighting)
  • Signal lighting housings (e.g., brake lights, indicators)
  • Durable transparent covers for sensors/electronics
  • UV-exposed exterior parts requiring color stability

Features & Benefits

Eco-Certified Recycled Content

This ISCC PLUS-attributed resin uses chemically recycled post-consumer materials, reducing environmental impact while meeting stringent automotive sustainability goals.

Superior Optical Performance

With 89% light transmittance (1mm) and <0.5% haze, it ensures crystal-clear lenses for headlamps, maintaining UV stability under harsh outdoor conditions.

Reliable Processing & Durability

Medium viscosity enables smooth injection molding (280–320°C), while high impact strength (70 kJ/m²) and 123°C heat deflection prevent warping/cracking in demanding applications.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top