Covestro Makrolon® 6267 X

Makrolon PC Polycarbonate

Makrolon 6267 X PC Resin Flame Retardant

Makrolon® 6267 X is a flame-retardant, low-viscosity polycarbonate resin with UL 94V-0 certification (1.5mm). Its easy-release properties, UV stabilization, and 19 cm³/10 min flow rate (300°C/1.2 kg) simplify injection molding of opaque safety-critical components like electrical housings.

  • Character: flame retardant; MVR (300 °C/1.2 kg) 19 cm³/10 min; UL 94V-0/1.5 mm; low viscosity; UV stabilized; easy release; available in opaque colors only
  • Application: Injection molding
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Flame Safety: UL 94V-0 (1.5mm), Glow Wire Test 960°C (3.0mm).
  • Flow & Shrinkage: MVR 19 cm³/10 min (300°C/1.2 kg); Mold Shrinkage 0.5–0.7%.
  • Tensile Modulus: 2,450 MPa
  • Flexural Strength: 97 MPa
  • Notched Impact (23°C): 60 kJ/m² (Charpy)
  • Thermal Stability: HDT 122°C (1.8 MPa); Vicat Softening 145°C.
  • Electrical Safety: CTI 225; Volume Resistivity 1E14 Ω·m.
  • Processing: Melt Temp 280–320°C; Dry 2–3 hrs at 120°C.

Application

  • Flame-Safe Electricals: Circuit breakers, switchgear housings.
  • Automotive Electronics: EV battery covers, sensor modules.
  • Industrial Hardware: Machine guards, tool housings.
  • Consumer Tech: Power adapters, LED lighting components.

Features & Benefits

Flame Retardancy & Safety Compliance

UL 94V-0 rated at 1.5mm and oxygen index of 36%, this pc makrolon 6267 x prevents fire spread in high-risk settings. Ideal for electrical enclosures in public spaces.

Low Viscosity & Easy Processing

With MVR 19 cm³/10 min, Makrolon® 6267 X fills complex molds effortlessly. Reduces cycle times and energy use for cost-efficient mass production.

Robust Mechanical Performance

67 MPa yield stress and 60 kJ/m² impact strength ensure durability. Perfect for automotive or industrial parts facing drops/vibration.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity