Covestro Makrolon® Rx1805 RE

Makrolon PC Polycarbonate

Makrolon Rx1805 RE PC Resin

Covestro PC Makrolon Rx1805 RE is a medical-grade, transparent polycarbonate resin with high viscosity (6.0 cm³/10 min MVR) and lipid resistance. It’s biocompatible, withstands radiation sterilization, and offers renewable ISCC PLUS mass balance attribution—ideal for demanding medical and chemical-resistant applications.

  • Character: MVR (300 °C/1.2 kg) 6.0 cm³/10 min; high viscosity; high lipid resistance; suitable for sterilization with high-energy radiation; biocompatible; Medical, CQ renewable attributed, Transparent, Chemical resistant
  • Application: Injection molding; Medical devices; Transparent parts for medical devices
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flow Rate: 6.0 cm³/10 min (300°C/1.2 kg)
  • Mechanical Strength: Tensile Modulus 2400 MPa, Impact Strength 80 kJ/m² (23°C notched)
  • Thermal Performance: HDT 138°C (1.8 MPa), Continuous Use: 120°C
  • Safety Compliance: Biocompatible, ≤0.02% moisture after drying
  • Processing: Melt Temp 290–330°C, Mold Temp 80–120°C
  • Density: 1200 kg/m³, Shrinkage 0.6–0.8%

Application

  • Medical Devices: Surgical instruments, IV connectors, dialysis housings.
  • Sterilization-Ready Components: Autoclavable trays, ETO-compatible seals.
  • Industrial Molding: Chemical-resistant labware, transparent covers for diagnostics.

Features & Benefits

Sustainable Medical Compliance

This ISCC PLUS-certified resin uses bio-circular raw materials via mass balance, reducing carbon footprint while meeting strict medical safety standards (ISO 10993-1). Buyers gain eco-compliance without sacrificing performance.

Unmatched Sterilization Durability

It withstands high-energy radiation, steam (121°C), and ETO sterilization without degradation. Ensures longevity for reusable medical devices, cutting replacement costs.

High Chemical & Impact Resistance

Exceptional lipid/oil resistance (puncture energy: 70J at -30°C) and transparency. Ideal for surgical tools, lab equipment, and transparent housings exposed to harsh fluids.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top