Covestro Makrolon® 1804 PC Resin

Makrolon PC Polycarbonate

Makrolon 1804 PC Resin Flame Retardant Grade

Covestro’s Makrolon 1804 is a high-viscosity, flame-retardant polycarbonate resin optimized for extrusion. With MVR 6.0 cm³/10 min (300°C/1.2kg), UL 94V-2 ratings (1.5mm/3.0mm), UV stabilization, and low plate-out, it delivers durable, transparent solid sheets for demanding industrial applications.

  • Character: flame retardant; MVR (300 °C/1.2 kg) 6.0 cm³/10 min; UL 94V-2/1.5 mm and 3.0 mm; high viscosity; UV stabilized; optimized for low plate-out; Transparent
  • Application: Extrusion; Solid sheet; Aircraft construction; Automotive construction; Railway construction
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flame Safety: UL 94 V-2 (1.5mm/3.0mm), V-0 (6.0mm); Oxygen Index 31%.
  • Strength & Durability: Tensile modulus 2400 MPa, yield stress 65 MPa, and >50% strain at break.
  • Thermal Resilience: HDT 127°C (1.8 MPa); Vicat softening 149°C.
  • Electrical Safety: CTI 225, volume resistivity 1E14 Ω·m.
  • Optical Clarity: 89% luminous transmittance (1mm); haze <0.8% (3mm).
  • Processing: Melt temp 300°C, mold temp 80°C; density 1200 kg/m³.

Application

  • Extrusion: High-clarity solid sheets for barriers or covers.
  • Aircraft Construction: Cabin interiors, lightweight window liners.
  • Automotive Construction: Dash components, lighting covers.
  • Railway Construction: Seat backs, impact-resistant partitions.

Features & Benefits

Reliable Flame Retardancy & Safety

Makrolon 1804 meets UL 94 V-2 (1.5mm/3.0mm) and V-0 (6.0mm), plus an oxygen index of 31%. Ideal for fire-sensitive environments like transport interiors, ensuring compliance without sacrificing transparency.

Extreme Impact Resistance

It boasts Charpy notched impact up to 80 kJ/m² (23°C) and puncture energy of 70 J (30°C). Perfect for high-stress parts like aircraft seating or automotive panels, reducing cracks and replacements.

Low-Maintenance Extrusion Performance

UV-stabilized and low plate-out design ensures consistent color and clarity in sheets. Minimizes equipment cleaning downtime, boosting production efficiency for solid sheet manufacturers.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top