Apec 2097 PC Resin Heat Resistant Grade
Covestro Apec® 2097 is a high-heat, UV-stabilized copolycarbonate resin engineered for demanding applications. With exceptional flow (MVR 8 cm³/10 min), easy-release properties, and a Vicat softening temperature of 202°C, it delivers reliability for precision injection-molded components like automotive lighting.
- Character: Copolycarbonate; MVR (330 °C/2.16 kg) 8 cm³/10 min; high viscosity; easy release; UV stabilized; softening temperature (VST/B 120) = 202 °C; Heat resistant
- Application: Injection molding; Lamp covers; Headlamp lenses
Key technical data (ISO)
- Vicat Softening Temp (VST/B 120): 202°C
- Heat Deflection Temp (1.8 MPa): 172°C | (0.45 MPa): 191°C
- Max Continuous Use Temp (UL): 150°C
- Tensile Modulus: 2,400 MPa
- Flexural Strength: 110 MPa
- Impact Resistance: Non-break at 23°C/-30°C (ISO 179)
- Light Transmittance: 89% (1mm thickness)
- Refractive Index: 1.566
- Melt Temp Range: 330–340°C
- Mold Temp: 130–150°C
- Drying: 130°C for 2–3 hrs (<0.02% moisture)
Application
- Automotive headlamp lenses and fog light covers
- Interior/exterior lamp housings and covers
- Precision injection-molded optical components
Features & Benefits
Related Apec® PC Resin Products
Covestro Apec® 1897 PC Resin
Covestro Apec® 1895 PC Resin
Covestro Apec® 1803 PC Resin
Covestro Makrolon® 1804 PC Resin
Covestro Makrolon® Rx1805 RE
Covestro Makrolon® 2858 RE
Covestro Makrolon® 2658 RE
Covestro Makrolon® 2458 RE
Covestro Makrolon® 2258 RE
Covestro Makrolon® Rx2530
Covestro Makrolon® Rx1851
Covestro Makrolon® Rx1805
Covestro Makrolon® Rx1452
Covestro Makrolon® 3158 PC Resin
Covestro Makrolon® 2658 PC Resin
Covestro Makrolon® 2558 PC Resin
Covestro Makrolon® 2258 PC Resin
Covestro Makrolon® 6267 X RE CQ
Advanced Manufacturing