Covestro Bayblend® T80 XG

Covestro Bayblend PC ABS blend

Bayblend® T80 XG PC/ABS Resin

Bayblend T80 XG by Covestro is a high-flow PC/ABS blend engineered for metallization (e.g., chrome plating). With a Vicat softening temperature of 130°C, excellent impact resistance, and optimized surface quality, it’s ideal for demanding automotive, electronics, and consumer goods.

  • Character:
  • Application:
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Vicat Softening Temp (B120): 130°C
  • Deflection Temp (1.8 MPa): 108°C
  • Tensile Modulus: 2,500 MPa
  • Notched Impact (23°C): 42 kJ/m²
  • Melt Flow Rate (260°C/5kg): 27 cm³/10min
  • Recommended Melt Temp: 260–280°C
  • UL94 Rating (0.85mm): HB
  • Density: 1.14 g/cm³
  • Dust Explosion Risk: Avoid fine dust accumulation

Application

  • Automotive: Grilles, emblems, interior trim.
  • Electronics: Laptop bezels, charger housings.
  • Consumer Goods: Power tool casings, premium appliance components.
  • Industrial: Connectors, control panels.

Features & Benefits

Perfect for Plated Surfaces

Optimized for steam-treated metallization, this Covestro PC/ABS Bayblend T80 XG ensures flawless chrome finishes without blisters—ideal for automotive grilles and appliance trims.

Effortless High-Speed Molding

With a melt flow rate of 27 cm³/10min (260°C/5kg), it fills complex molds quickly, reducing cycle times and energy costs for thin-walled electronics housings.

Toughness Meets Precision

It delivers 42 kJ/m² notched impact strength at 23°C and low molding shrinkage (0.55–0.75%), ensuring durable, dimensionally stable parts like power tools and connectors.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top